Material Notes:
Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinability; Dimensional Stability; Excellent Weldability; High Strength to Weight Ratio; Enhanced Corrosion Resistance; Ultrasonically Inspected; Gauge 2” - 38”; widths up to 94". Surface Condition & Roughness: Machined 2 Sides (25 RMS) Sawed Surface (+.125”/-0)
Physical Properties Metric English Comments
Density 2.66 g/cc
0.0960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
Tensile Strength, Ultimate 283 MPa
41000 psi
Tensile Strength, Yield 124 MPa
18000 psi
Elongation at Break 12 - 15 %
12 - 15 %
in 2"
Modulus of Elasticity 69.6 GPa
10100 ksi
Thermal Properties Metric English Comments
CTE, linear 23.6 µm/m-°C

@Temperature 20.0 - 100 °C
13.1 µin/in-°F

@Temperature 68.0 - 212 °F
24.1 µm/m-°C

@Temperature 101 - 200 °C
13.4 µin/in-°F

@Temperature 213 - 392 °F
Thermal Conductivity 140 W/m-K
972 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000059 ohm-cm
0.0000059 ohm-cm