Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Arkema
Trade Name LOTADER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reactivity, softness), LOTADER® AX 8900 is an additive (toughener) of choice in order to improve the impact strength of engineering thermoplastics like PA, Polyesters (PBT, PET), PC/PBT and PC/ABS alloys, PPS. It can also be use as a compatibilizer for Polyesters/Polyolefins blends and as an adhesive for some laminate structures.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 24 %
24 %
FTIR (internal)
Melt Index of Compound 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
ASTM D2240
Hardness, Shore D 18
18
ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Modulus of Elasticity 0.00800 GPa
1.16 ksi
ASTM D638
Flexural Modulus <= 0.0300 GPa
<= 4.35 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 65.0 °C
149 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 0.999 kg
<= 104 °F

@Load 2.20 lb
ASTM D1525
Descriptive Properties Value Comments
Glycidyl Methacrylate Content (%) 8
FTRI (internal)