Polymer Property : Tensile Impact Strength = 1.19 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 2.50 - 945 kJ/m²
1.19 - 450 ft-lb/in²
Average value: 536 kJ/m² Grade Count:17
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Tensile Impact Strength 2.50 kJ/m²
1.19 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-612 EVA Injection Molding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This re..