Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 2.50 - 945 kJ/m² | 1.19 - 450 ft-lb/in² | Average value: 536 kJ/m² Grade Count:17 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |