Tensile Impact Strength 2.50 - 945 kJ/m²
1.19 - 450 ft-lb/in²
Average value: 536 kJ/m² Grade Count:17
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..