Mechanical Properties Metric English Comments
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21540 Coax & Telecom Flexible PVC
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi..
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21540 Coax & Telecom Flexible PVC Black 307
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C ..
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21570 Coax & Telecom Flexible PVC
Semi-rigid insulation compound designed for data communication riser cable applications. Maximum 75°C service temperature rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp..