Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.0190 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Precision Polymer Engineering Perlast® G90A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat..
100% Modulus 0.0190 GPa
2.76 ksi
ISO 37
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..
100% Modulus 0.0190 GPa
2.76 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and ..
100% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21540 Coax & Telecom Flexible PVC
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi..
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21540 Coax & Telecom Flexible PVC Black 307
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C ..
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Axiall 21570 Coax & Telecom Flexible PVC
Semi-rigid insulation compound designed for data communication riser cable applications. Maximum 75°C service temperature rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp..
100% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Copyright © lookpolymers.com All Rights Reserved