Axiall 19880 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19880 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
105°C rated, 30 mil and larger, clear compound recommended for VW-1 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.27 g/cc
1.23 - 1.27 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 91
85 - 91
delayed; ASTM D-2240
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Elongation at Yield 257.6 %
257.6 %
Air Aging: 7 days @ 136°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 26 %
26 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F