BASF Palatinol® 11P-E (DUP) Linear Phthalate

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Palatinol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Palatinol® 11P-E (DUP) Linear Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing characteristics with vinyl resin. Its viscosity is relatively low in relation to its molecular weight. Palatinol 11P-E is inhibited with 0.1% by weight of 1,1,3-tris(2-methyl-4-hydroxy 5-t butylphenyl) butane.Applications: Vinyl resin compounders choose Palatinol 11P-E over DTDP for its lower viscosity, greater resin compatibility, faster dry blending and superior efficiency. When formulated to equal concentrations, Palatinol 11P-E provides equal electrical properties in 90°C and 105°C wire insulation compounds. With its lower viscosity, high thermal resistance, permanence and low volatility, Palatinol 11P-E is well suited for demanding applications such as automotive interior (instrument panel skins), building wire insulation, 90° THW and 105° THW, automotive wire harness and vinyl roofing membrane.Information provided by BASF
Physical Properties Metric English Comments
Density 0.948 - 0.955 g/cc
0.0342 - 0.0345 lb/in³
ASTM D4052
Solubility of Water 0.0015 %
0.0015 %
Solubility in Water <= 1.0e-6 %
<= 1.0e-6 %
Viscosity 27 cP

@Temperature 40.0 °C
27 cP

@Temperature 104 °F
Absolute
71 cP

@Temperature 20.0 °C
71 cP

@Temperature 68.0 °F
Absolute
255 cP

@Temperature 0.000 °C
255 cP

@Temperature 32.0 °F
Absolute
Molecular Weight 474 g/mol
474 g/mol
Vapor Pressure <= 0.000800 bar
<= 0.600 torr
Mechanical Properties Metric English Comments
Hardness, Shore A 76

@Time 15.0 sec
76

@Time 0.00417 hour
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
88

@Time 15.0 sec
88

@Time 0.00417 hour
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
93

@Time 15.0 sec
93

@Time 0.00417 hour
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 14.8 MPa
2150 psi
Plasticizer conc. in vinyl film 70 phr; ASTM D638
18.5 MPa
2680 psi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
20.6 MPa
2990 psi
Plasticizer conc. in vinyl film 40 phr; ASTM D638
Elongation at Break 255 %
255 %
Plasticizer conc. in vinyl film 40 phr; ASTM D638
285 %
285 %
Plasticizer conc. in vinyl film 50 phr; ASTM D638
325 %
325 %
Plasticizer conc. in vinyl film 70 phr; ASTM D638
100% Modulus 0.00793 GPa
1.15 ksi
Plasticizer conc. in vinyl film 70 phr; ASTM D638
0.0121 GPa
1.75 ksi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
0.0165 GPa
2.39 ksi
Plasticizer conc. in vinyl film 40 phr; ASTM D638
Torsional Stiffness 310 MPa

@Temperature -15.0 °C
45000 psi

@Temperature 5.00 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
310 MPa

@Temperature -30.0 °C
45000 psi

@Temperature -22.0 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
310 MPa

@Temperature -45.0 °C
45000 psi

@Temperature -49.0 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
Thermal Properties Metric English Comments
CTE, linear 790 µm/m-°C
439 µin/in-°F
Boiling Point 262 °C

@Pressure 1.32e+6 MPa
504 °F

@Pressure 1.91e+8 psi
Pour Point -9.00 °C
15.8 °F
Brittleness Temperature -50.0 °C
-58.0 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D746
-42.0 °C
-43.6 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D746
-32.0 °C
-25.6 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D746
Flash Point 254 °C
489 °F
Optical Properties Metric English Comments
Refractive Index 1.481
1.481
Chemical Properties Metric English Comments
Total Acid Number <= 0.10
<= 0.10
[mg KOH/g]; ASTM D1045
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
ASTM E203
Descriptive Properties Value Comments
Color <50
APAH, ASTM D5386
Composition Ester content
>99.6%, ASTM D3465