Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Nordel® IP 4640 Dense Extruded Profile

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® IP 4640 Dense Extruded Profile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationNordel® IP 4640
Physical Properties Metric English Comments
Density 1.185 g/cc
0.04281 lb/in³
Mooney Viscosity 37

@Temperature 100 °C
37

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 8.30 MPa
1200 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 330 %
330 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00310 GPa
0.450 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00670 GPa
0.972 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00800 GPa
1.16 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 31.6 kN/m
180 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 90 %

@Temperature 125 °C
90 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -38.0 °C
-36.4 °F
Temperature Retraction, TR-10