Mechanical Properties Metric English Comments
100% Modulus 0.00160 GPa
0.232 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica..
100% Modulus 0.00160 GPa
0.232 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00160 GPa
0.232 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00160 GPa
0.232 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00160 GPa
0.232 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00160 GPa
0.232 ksi
ISO 37
ELASTO UK Dryflex® 3038-111 TPE, Modified Injection Molding Grade for Auto Interior Parts
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3038-111 is specifically designe..
100% Modulus 0.00160 GPa
0.232 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4520 Molded Golf Grip
FormulationNordel® IP 4520
100% Modulus 0.00160 GPa
0.232 ksi
ISO 37
AlphaGary Evoprene™ 089 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
100% Modulus 0.00160 GPa
0.232 ksi
ISO 37
AlphaGary Evoprene™ 084 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..