Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00160 GPa | 0.232 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica.. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | ISO 37 |
ELASTO UK Dryflex® 3038-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3038-111 is specifically designe.. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 Molded Golf Grip FormulationNordel® IP 4520 |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | ISO 37 |
AlphaGary Evoprene™ 089 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00160 GPa | 0.232 ksi | ISO 37 |
AlphaGary Evoprene™ 084 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |