Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Dryflex® 3038-111 TPE, Modified Injection Molding Grade for Auto Interior Parts

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 3038-111 TPE, Modified Injection Molding Grade for Auto Interior Parts.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3038-111 is specifically designed for auto interior parts such as mats.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 2781
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 230 °C
25 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
ISO 868
Tensile Strength at Break 6.10 MPa
885 psi
ISO 37
Elongation at Break 670 %
670 %
ISO 37
100% Modulus 0.00160 GPa
0.232 ksi
ISO 37
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: