TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5N-550 Black30.0TP-9520.0Akrofax 7585.0Di-Cup 40C2.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 17.31 MPa
2511 psi
Elongation at Yield 491 %
491 %
100% Modulus 0.00150 GPa
0.218 ksi
200% Modulus 0.00412 GPa
0.598 ksi
300% Modulus 0.007812 GPa
1.133 ksi
Tear Strength 42.2 kN/m
241 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 160 °C
0.250 hour

@Temperature 320 °F
Users viewing this material also viewed the following: