Polymer Property : 100% Modulus = 0.00200 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00120 - 0.00200 GPa
0.174 - 0.290 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
100% Modulus 0.00150 - 0.00200 GPa
0.218 - 0.290 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..