Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00793 GPa | 1.15 ksi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00793 GPa | 1.15 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5660Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5660Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
100% Modulus | 0.00793 GPa | 1.15 ksi | ASTM D-638 |
Axiall 16860 Wire & Cable Flexible PVC Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00793 GPa | 1.15 ksi | ASTM D-638 |
Axiall 1751 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
100% Modulus | 0.00793 GPa | 1.15 ksi | Plasticizer conc. in vinyl film 70 phr; ASTM D638 |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |
|||
100% Modulus | 0.00793 GPa | 1.15 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |