Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 1.15 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D412
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound
Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers
100% Modulus 0.00790 GPa
1.15 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or..
100% Modulus 0.00790 GPa
1.15 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00790 GPa
1.15 ksi
Heat aged 2 weeks at 175°C
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00793 GPa
1.15 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5660Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5660Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D-638
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D-638
Axiall 1751 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..
100% Modulus 0.00793 GPa
1.15 ksi
Plasticizer conc. in vinyl film 70 phr; ASTM D638
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing ..
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00790 GPa
1.15 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00790 GPa
1.15 ksi
DIN 53504
Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance
Introduction: IROGRAN A92K 4107 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c..
Copyright © lookpolymers.com All Rights Reserved