Mechanical Properties Metric English Comments
100% Modulus 0.00290 GPa
0.421 ksi
ISO/R527
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
100% Modulus 0.00290 GPa
0.420 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00290 GPa
0.421 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
100% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
100% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
100% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
100% Modulus 0.00290 GPa
0.420 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00290 GPa
0.420 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00290 GPa
0.421 ksi
JIS 6251 (Dumbbells)
DuPont Performance Polymers Kalrez® 8002 FFKM Perfluoroelastomer
Kalrez® 8002 is a specialty compound targeted specifically for select semiconductor plasma and gas deposition applications. This clear, unfilled compound offers very low particle generation in oxyg..
100% Modulus 0.00290 GPa
0.420 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00290 GPa
0.421 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..