Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
ASTM D412
Tensile Strength at Break 17.5 MPa
2540 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
100% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
200% Modulus 0.00740 GPa
1.07 ksi
ASTM D412
300% Modulus 0.0125 GPa
1.81 ksi
ASTM D412
Tear Strength 47.0 kN/m
268 pli
ASTM D2240
Copyright © lookpolymers.com All Rights Reserved