Polymer Property : Compressive Strength = 183 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 183 MPa
26500 psi
ASTM D695
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass
Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Compressive Strength 183 MPa
26500 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Plenco 4466 Phenolic, Granular, Transfer Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Plenco 4599 Phenolic, Granular, Injection Molded
PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated ..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Plenco 4504 Phenolic, Granular, Compression Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..
Compressive Strength 183 MPa
26500 psi
ASTM D695
Plenco 4548 Phenolic, Granular, Injection Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Compressive Strength 183 MPa
26600 psi
ASTM D695
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..