Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 112 MPa | 16200 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Compressive Strength | 112 MPa | 16200 psi | Perpendicular |
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Compressive Strength | 112 MPa | 16200 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Compressive Strength | 112 MPa | 16200 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Compressive Strength | 112 MPa | 16200 psi | break; DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Compressive Strength | 112 MPa | 16200 psi | |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |
|||
Compressive Strength | 112 MPa | 16200 psi | ASTM D695 |
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin.. |
|||
Compressive Strength | 112 MPa | 16200 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |