Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpire AV-650. It has been specifically formulated for applications requiring a balance of chemical resistance and mechanical strength along with good part aesthetics, bridging the performance gaps within the ultra polymers space. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. AvaSpire AV-651 can be easily processed by typical injection molding and extrusion methods using conventional processing equipment. - Natural: AvaSpire AV-651 NT - Beige: AvaSpire AV-651 BG 15Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Viscosity 240000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
240000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.18 mm
0.0070 - 0.0090 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm

@Thickness 3.18 mm
0.010 - 0.012 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 400 °C
25 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
M-Scale; ASTM D785
Tensile Strength 87.0 MPa
12600 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 89.0 MPa
12900 psi
ISO 527-2/1A/50
Elongation at Break >= 40 %
>= 40 %
50 mm/min; ASTM D638
>= 40 %
>= 40 %
ISO 527-2/1A/50
Elongation at Yield 5.7 %
5.7 %
ISO 527-2/1A/50
6.2 %
6.2 %
50 mm/min; ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
50 mm/min; ASTM D638
3.20 GPa
464 ksi
ISO 527-2/1A/1
Flexural Strength 124 MPa
18000 psi
ASTM D790
127 MPa
18400 psi
ISO 178
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
3.20 GPa
464 ksi
ISO 178
Compressive Strength 112 MPa
16200 psi
ASTM D695
Shear Strength 78.0 MPa
11300 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
NB
NB
ASTM D256
Izod Impact, Notched (ISO) 6.60 kJ/m²
3.14 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 47.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
26.1 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Specific Heat Capacity 1.31 J/g-°C

@Temperature 50.0 °C
0.313 BTU/lb-°F

@Temperature 122 °F
DSC
1.82 J/g-°C

@Temperature 200 °C
0.435 BTU/lb-°F

@Temperature 392 °F
DSC
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM E1530
Melting Point 345 °C
653 °F
Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 3.20 mm
374 °F

@Thickness 0.126 in
Annealed; 2 hours at 200°C; ASTM D648
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+17 ohm-cm
5.00e+17 ohm-cm
ASTM D257
Surface Resistance >= 1.90e+17 ohm
>= 1.90e+17 ohm
ASTM D257
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
ASTM D150
3.1

@Frequency 60.0 Hz
3.1

@Frequency 60.0 Hz
ASTM D150
3.12

@Frequency 1000 Hz
3.12

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm

@Thickness 3.00 mm
406 kV/in

@Thickness 0.118 in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0010

@Frequency 60.0 Hz
0.0010

@Frequency 60.0 Hz
ASTM D150
0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 355 °C
671 °F
Middle Barrel Temperature 365 °C
689 °F
Front Barrel Temperature 370 °C
698 °F
Nozzle Temperature 375 °C
707 °F
Melt Temperature 365 - 390 °C
689 - 734 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 150 °C
302 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Agency Ratings ISO 10993
ISO 10993-Part 1
Appearance Beige
Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Autoclave Sterilizable
Biocompatible
Ductile
E-beam Sterilizable
Ethylene Oxide Sterilizable
Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Impact Resistance
Good Sterilizability
Heat Sterilizable
High Heat Resistance
Radiation (Gamma) Resistant
Radiation Sterilizable
Radiotranslucent
Steam Resistant
Steam Sterilizable
Forms Pellets
Generic PAEK
Injection Rate Fast
Processing Method Extrusion Blow Molding
Fiber (Spinning) Extrusion
Film Extrusion
Injection Blow Molding
Injection Molding
Machining
Profile Extrusion
Thermoforming
Wire & Cable Extrusion
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0 to 3.0:1.0
Uses Aerospace Applications
Aircraft Applications
Bearings
Dental Applications
Film
Hospital Goods
Industrial Applications
Medical Appliances
Medical/Healthcare Applications
Oil/Gas Applications
Pump Parts
Seals
Surgical Instruments
Users viewing this material also viewed the following: