Polymer Property : Compressive Strength = 14000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 68.95 - 96.53 MPa
10000 - 14000 psi
after 816°C
Pyrotek Pyrocast ZI Refractory Shapes
Aggregate Base: BauxiteApplicationsCrucible bottoms Information provided by Pyrotek.
Compressive Strength 68.95 - 96.53 MPa
10000 - 14000 psi
after 816°C
Pyrotek Pyrocast ZC Refractory Shapes
Aggregate Base: MulliteApplicationsDoor sill Breech plug Door jamb Information provided by Pyrotek.
Compressive Strength 68.95 - 96.53 MPa
10000 - 14000 psi
after 816°C
Pyrotek Pyrocast ZR Refractory Shapes
Aggregate Base: Fused Silica / MulliteApplicationsTransfer troughs Information provided by Pyrotek.
Compressive Strength 82.7 - 96.5 MPa
12000 - 14000 psi
ASTM D695
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Compressive Strength 82.7 - 96.5 MPa
12000 - 14000 psi
ASTM D695
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6
NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Compressive Strength 68.95 - 96.53 MPa
10000 - 14000 psi
after 816°C
Pyrotek Pyrocast ZA Refractory Shapes
Aggregate Base: Mullite / SiCApplicationsWear Pads TCPT's Information provided by Pyrotek.