Pyrotek Pyrocast ZC Refractory Shapes

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast ZC Refractory Shapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aggregate Base: MulliteApplicationsDoor sill Breech plug Door jamb Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.74 g/cc
0.0990 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 68.95 - 96.53 MPa
10000 - 14000 psi
after 816°C
Abrasion 4.0 - 8.0
4.0 - 8.0
Resistance (CC Loss) ASTM C704
Thermal Properties Metric English Comments
CTE, linear 6.12 µm/m-°C

@Temperature 20.0 °C
3.40 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.67 W/m-K

@Temperature 538 °C
11.6 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Maximum Service Temperature, Air 1649 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 63.5 %
63.5 %