Polymer Property : Compressive Strength = 96.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 82.7 - 96.5 MPa
12000 - 14000 psi
ASTM D695
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Compressive Strength 82.7 - 96.5 MPa
12000 - 14000 psi
ASTM D695
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6
NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..