Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the excellent flow and controlled reactivity, BMC A30-3021 is well suited for injection, transfer or compression molding.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.84 - 2.04 g/cc
0.0665 - 0.0737 lb/in³
Molded
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
0.00050 - 0.0015 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 33.1 - 46.9 MPa
4800 - 6800 psi
Flexural Strength 82.7 - 110 MPa
12000 - 16000 psi
Flexural Modulus 6.89 - 8.27 GPa
1000 - 1200 ksi
Compressive Strength 93.1 - 121 MPa
13500 - 17500 psi
Izod Impact, Notched 1.60 - 3.20 J/cm
3.00 - 6.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 10.8 - 12.8 kV/mm
275 - 325 kV/in
short time
Arc Resistance >= 180 sec
>= 180 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F