Description: Good mold release, excellent part finish (low bloom).Applications: Suggested uses include housewares, caps and closures, mugs / cups, thin-walled containers.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
2 in/min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256A