Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.0 - 35.0 MPa | 2180 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Tensile Strength | 20.0 - 35.0 MPa | 2900 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Tensile Strength | 25.0 - 35.0 MPa | 3630 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Tensile Strength | 15.0 - 35.0 MPa | 2180 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Tensile Strength | 20.0 - 35.0 MPa | 2900 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Tensile Strength | 25.0 - 35.0 MPa | 3630 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Tensile Strength | 30.0 - 35.0 MPa | 4350 - 5080 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm.. |
|||
Tensile Strength | 30.0 - 35.0 MPa | 4350 - 5080 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion.. |
|||
Tensile Strength | 27.0 - 35.0 MPa | 3920 - 5080 psi | ISO 527 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Tensile Strength | 30.0 - 35.0 MPa | 4350 - 5080 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |