Mechanical Properties Metric English Comments
Tensile Strength 15.0 - 35.0 MPa
2180 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..
Tensile Strength 20.0 - 35.0 MPa
2900 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -..
Tensile Strength 25.0 - 35.0 MPa
3630 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
Tensile Strength 15.0 - 35.0 MPa
2180 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..
Tensile Strength 20.0 - 35.0 MPa
2900 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -..
Tensile Strength 25.0 - 35.0 MPa
3630 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
Tensile Strength 30.0 - 35.0 MPa
4350 - 5080 psi
ISO 527
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound
Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm..
Tensile Strength 30.0 - 35.0 MPa
4350 - 5080 psi
ISO 527
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
Tensile Strength 27.0 - 35.0 MPa
3920 - 5080 psi
ISO 527
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Tensile Strength 30.0 - 35.0 MPa
4350 - 5080 psi
ISO 527
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..