Dalau Dalcon 001 100% Virgin PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dalau Dalcon 001 100% Virgin PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carrying chemicals; and Seals & gaskets. Flat gaskets are used to seal flanges in pipelines.Construction: Bridge bearings. Slide bearings.Electrical: Communications, radio & television engineering, cable insulation; Electrical plant construction & electronics industry (connectors & terminals); General electrical equipment (P.T.F.E. excellent electrical insulating material); and Power plant installations (switchgear).Engineering: Anti - friction bearing cages & bearing plates; Bearings and bushes; Diaphragm pumps. Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology; Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.Food: Dynamic & shaft seals (used in the food processing industry) and Linings & coatings (fertiliser plant & food industry line equipment).CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, and some fluorine compounds at elevated temperatures. Some Fluorinated Hydrocarbons (refrigerants) cause reversible swelling i.e. Tetrafluorodichloroethane Frigen 21, giving a 9.6% weight increase. For specific data on chemical resistance of this material we have a computer database with all the information covering over 90% of all known chemicals.Information provided by Dalau
Physical Properties Metric English Comments
Density 2.13 - 2.19 g/cc
0.0770 - 0.0791 lb/in³
BS2782:Pt6
Deformation 7.9 %
7.9 %
Permanent Deformation; ASTM D621
10 %

@Time 3600 sec,
Pressure 5.00 MPa
10 %

@Time 1.00 hour,
Pressure 725 psi
150°C; ASTM D621
11.8 %

@Time 3600 sec,
Pressure 14.2 MPa
11.8 %

@Time 1.00 hour,
Pressure 2060 psi
ASTM D621
14.3 %

@Pressure 14.2 MPa,
Time 86400 sec
14.3 %

@Pressure 2060 psi,
Time 24.0 hour
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 64
57 - 64
ASTM D2240
Tensile Strength 15.0 - 35.0 MPa
2180 - 5080 psi
Moulding Direction; BS2782:Pt3
Elongation at Break 150 - 350 %
150 - 350 %
Moulding Direction; BS2782:Pt3
Flexural Modulus 0.690 GPa
100 ksi
ASTM D790
Compressive Modulus 0.600 - 0.700 GPa

@Strain 0.200 %
87.0 - 102 ksi

@Strain 0.200 %
ASTM D621
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 142 µm/m-°C

@Temperature 23.0 - 200 °C
78.9 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
CTE, linear, Transverse to Flow 153 µm/m-°C

@Temperature 23.0 - 200 °C
85.0 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Melting Point 327 °C
621 °F
ASTM D3417
Maximum Service Temperature, Air 260 °C
500 °F
300 °C
572 °F
Short Periods
Minimum Service Temperature, Air -200 °C
-328 °F
Flash Point 530 °C
986 °F
ASTM D1929
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Optical Properties Metric English Comments
Haze 80 - 85 %
80 - 85 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Dielectric Constant 2.1

@Frequency 60.0 Hz
2.1

@Frequency 60.0 Hz
ASTM D150
2.1

@Frequency 1.00e+6 Hz
2.1

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
610 kV/in
Oil(Molding); ASTM D149
35.0 kV/mm
889 kV/in
Oil (Extrusion); ASTM D149
60.0 - 80.0 kV/mm
1520 - 2030 kV/in
Air (Tape); ASTM D149
Dissipation Factor <= 0.00030

@Frequency 60.0 Hz
<= 0.00030

@Frequency 60.0 Hz
ASTM D150
<= 0.00030

@Frequency 1.00e+6 Hz
<= 0.00030

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Color White