Tensile Strength 276 MPa
40000 psi
ASTM D638
PlastiComp Complet® LCF30-PA66 30% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Strength 276 MPa
40000 psi
ASTM D-638
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Tensile Strength 276 MPa
40000 psi
ASTM D638
PlastiComp Complet® LCF40-PA66 40% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Strength 276 - 552 MPa
40000 - 80000 psi
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength 276 - 607 MPa
40000 - 88000 psi
Chicago Extruded Metals UNS C34000 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength 276 - 1030 MPa
40000 - 150000 psi
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength 276 - 552 MPa
40000 - 80000 psi
Chicago Extruded Metals UNS C35000 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals
Tensile Strength 276 - 552 MPa
40000 - 80000 psi
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals
Tensile Strength 276 - 552 MPa
40000 - 80000 psi
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength 276 - 621 MPa
40000 - 90000 psi
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal..
Tensile Strength 276 - 669 MPa
40000 - 97000 psi
Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal..
Tensile Strength 276 - 552 MPa
40000 - 80000 psi
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals