Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LCF30-PA66 30% Long Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30-PA66 30% Long Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 276 MPa
40000 psi
ASTM D638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D638
Tensile Modulus 22.76 GPa
3301 ksi
ASTM D638
Flexural Strength 359 MPa
52100 psi
ASTM D790
Flexural Modulus 16.55 GPa
2400 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.68 J/cm
20.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
ASTM D648
Users viewing this material also viewed the following: