Material Notes:
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 42
42
Tensile Strength 276 - 621 MPa
40000 - 90000 psi
Elongation at Break 3.0 - 50 %
3.0 - 50 %
Machinability 20 %
20 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 89 - 91 %
89 - 91 %
Iron, Fe 0.050 %
0.050 %
Lead, Pb 0.050 %
0.050 %
Other, total 0.20 %
0.20 %
Zinc, Zn 8.7 - 10.7 %
8.7 - 10.7 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000391 ohm-cm
0.00000391 ohm-cm