Polymer Property : Tensile Strength = 132 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 132 MPa
19100 psi
ASTM D638
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin
Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon.
Tensile Strength 132 MPa
19200 psi
ASTM D638
Gromax PBT 4140-201D 40% Glass Fiber Filled
Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Tensile Strength 132 MPa
19200 psi
50 mm/min; ISO 527-1,-2
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 132 MPa
19200 psi
50 mm/min; ISO 527
Gromax BTG30-FN03N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 132 MPa
19200 psi
ASTM D638
Samyang Tramid® 210G15 Polyamide, Reinforced
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectors..
Tensile Strength 132 MPa
19200 psi
ASTM D638
Gromax CCP PBT 3040-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..