Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Kolon
Trade Name SPESIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.050 %
0.050 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 132 MPa
19100 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 8.826 GPa
1280 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM D696
Melting Point 224 °C
435 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.7
3.7
ASTM D150
Dielectric Strength 27.0 kV/mm
686 kV/in
ASTM D149
Arc Resistance 110 sec
110 sec
ASTM D495