Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectorsIntake manifoldsThermostat housingCooling radiator modulesSprinklerWater pipesFan and shroudECU casesCylinder head coverIndustrial ball valveInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.70 %
0.70 %
ASTM D570
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 132 MPa
19200 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 4.81 GPa
697 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 248 °C
478 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149