Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tygon S3™ E-LFL from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3™ line combines the high performance standards customers demand with an eco-friendly tubing design. The new Tygon S3™ E-LFL non-DEHP tubing is our best performing peristaltic pump tubing. Tygon S3™ E-LFL has been tested rigorously to ensure that it meets the same physical standards as the old Tygon® LFL tubing, including 1,000 hours of peristaltic pump tubing life at 0 psi back pressure, low particulate spallation and chemical resistance. Crystal-clear Tygon S3™ E-LFL tubing is formulated specifically for use in peristaltic pump applications. With its superior flex life characteristics, manufacturing processes can be simplified by reducing production downtime due to pump tubing failure. The excellent wear properties of Tygon S3™ E-Long Flex Life Pump Tubing also lead to a reduction of particulate spallation. This feature limits the risk of sensitive-fluid contamination critical to the pharmaceutical, cosmetic, food and beverage industries. Non-aging characteristics and broad chemical resistance provide users with versatility in use for a wide variety of applications. Safe and non-toxic Tygon S3™ E-Long Flex Life Pump Tubing can be produced in up to a 6" inside diameter, making it the ideal choice in bulk transfer applications. Applications Wide range of liquid transfer in labs Production filtration and fermentation Food & beverage and cosmetic processing Biopharmaceutical Surfactant delivery Flavor and vitamin concentrate dispensing Printing ink transfer Highly viscous fluid transfer Drum and tank drainage Shear-sensitive fluid transfer Features and Benefits Longest flex life of any clear Tygon® tubing -- reduces downtime due to pump failure Extremely low particulate spallation -- reliable for sensitive-fluid applications Broad chemical resistance -- excellent for laboratory applications Can be autoclaved -- suitable for high purity applications Contains no BPA or phthalate Regulatory Information: Tygon S3™ complies with FDA, NSF, 3-A, USP Class VI, ISO 10993, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EC for many foods and beverages. Tygon S3™ tubing products do not contain chemicals listed in California's Prop 65.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 22.8 °C,
Time 86400 sec
0.20 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 56

@Time 15.0 sec
56

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
Tensile Strength, Yield 3.79 MPa

@Strain 100 %
550 psi

@Strain 100 %
ASTM D412
6.55 MPa

@Strain 200 %
950 psi

@Strain 200 %
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Tear Strength 32.3 kN/m
184 pli
ASTM D1004
Compression Set 68 %

@Temperature 70.0 °C,
Time 79200 sec
68 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Tensile Set 54 %
54 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
temperature limit for flexibility
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
USP Class VI Yes
Yes
Descriptive Properties Value Comments
Color Clear