Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - K (Potassium) | 4.0 ppm | 4.0 ppm | |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Ionic Impurities - K (Potassium) | 4.0 ppm | 4.0 ppm | |
Epoxy Technology EPO-TEK® E2001-HV Electrically Conductive, Silver-Filled Epoxy Product Description: EPO-TEK® E2001-HV Is a snap cure, two component, silver-filled die attach adhesive for semiconductor plastic IC packaging.Advantages & Application Notes:Snap cure adhesive or f.. |
|||
Ionic Impurities - K (Potassium) | 4.0 ppm | 4.0 ppm | |
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Ionic Impurities - K (Potassium) | 4.0 ppm | 4.0 ppm | |
Epoxy Technology EPO-TEK® ED1020 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Its unique features include exce.. |
|||
Ionic Impurities - K (Potassium) | 4.0 ppm | 4.0 ppm | |
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two .. |