Polymer Property : Linear Mold Shrinkage, Flow = 0.0026 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0024 - 0.0026 cm/cm

@Time 86400 sec
0.0024 - 0.0026 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0017 - 0.0026 cm/cm

@Time 86400 sec
0.0017 - 0.0026 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66
LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
Linear Mold Shrinkage, Flow 0.0017 - 0.0026 cm/cm

@Time 86400 sec
0.0017 - 0.0026 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.