Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0024 - 0.0026 cm/cm

@Time 86400 sec
0.0024 - 0.0026 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12
LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS
LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA
LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS
LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific)
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.