Material Notes:
Production Method: A Grade - Glycol solution in water with mass fraction greater than 75% B Grade - Glycol solution in water with mass fraction greater than 45% Application: A Grade - Intended for making coolant liquids concentrate. B Grade - Intended for making coolant-cutting fluids.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 1.06 - 1.12 g/cc

@Temperature 20.0 °C
0.0383 - 0.0405 lb/in³

@Temperature 68.0 °F
B Grade
1.08 - 1.11 g/cc

@Temperature 20.0 °C
0.0390 - 0.0401 lb/in³

@Temperature 68.0 °F
A Grade, 2nd Quality
1.09 - 1.13 g/cc

@Temperature 20.0 °C
0.0394 - 0.0408 lb/in³

@Temperature 68.0 °F
A Grade, 1st Quality
Thermal Properties Metric English Comments
Minimum Service Temperature, Air <= -40.0 °C
<= -40.0 °F
Grade B
Component Elements Properties Metric English Comments
Free Water <= 3.0 %
<= 3.0 %
Grade A - 1 quality
<= 25 %
<= 25 %
Grade A - 2 quality
<= 55 %
<= 55 %
Grade B
Descriptive Properties Value Comments
Appearance Transparent or yellowish fluid
Mass Content (%) 25
Mass content of diethyleneglycol, Grade B
30
Mass content of ethyleneglycol, Grade B
45
Mass content of glycols including ethyleneglycol, diethyleneglycol, and triethyleneglycol, Grade B
5
Mass content of triethyleneglycol, Grade B
60
Mass content of ethyleneglycol, Grade A - 2 quality
75
Mass content of glycols including ethyleneglycol, diethyleneglycol, and triethyleneglycol, Grade A - 2 quality
92
Mass content of ethyleneglycol, Grade A - 1 quality
97
Mass content of glycols including ethyleneglycol, diethyleneglycol, and triethyleneglycol, Grade A - 1 quality
Copyright © lookpolymers.com All Rights Reserved