Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Epichlorohydrin

Category Fluid
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Epichlorohydrin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy applications, such as Pulp & paper chemicals, Water treatment and Healthcare products. Solvay has developed and patented a new glycerin-based process for the production of epichlorohydrin, called Epicerol®. EINECS Number: 203-439-8/CAS Number: 106-89-8/UN number: 2023Information provided by Solvay
Physical Properties Metric English Comments
Density 1.054 g/cc

@Temperature 120 °C
0.03808 lb/in³

@Temperature 248 °F
1.067 g/cc

@Temperature 110 °C
0.03855 lb/in³

@Temperature 230 °F
1.08 g/cc

@Temperature 100 °C
0.0390 lb/in³

@Temperature 212 °F
1.093 g/cc

@Temperature 90.0 °C
0.03949 lb/in³

@Temperature 194 °F
1.106 g/cc

@Temperature 80.0 °C
0.03996 lb/in³

@Temperature 176 °F
1.119 g/cc

@Temperature 70.0 °C
0.04043 lb/in³

@Temperature 158 °F
1.131 g/cc

@Temperature 60.0 °C
0.04086 lb/in³

@Temperature 140 °F
1.144 g/cc

@Temperature 50.0 °C
0.04133 lb/in³

@Temperature 122 °F
1.156 g/cc

@Temperature 40.0 °C
0.04176 lb/in³

@Temperature 104 °F
1.162 g/cc

@Temperature 35.0 °C
0.04198 lb/in³

@Temperature 95.0 °F
1.168 g/cc

@Temperature 30.0 °C
0.04220 lb/in³

@Temperature 86.0 °F
1.174 g/cc

@Temperature 25.0 °C
0.04241 lb/in³

@Temperature 77.0 °F
1.181 g/cc

@Temperature 20.0 °C
0.04267 lb/in³

@Temperature 68.0 °F
1.187 g/cc

@Temperature 15.0 °C
0.04288 lb/in³

@Temperature 59.0 °F
1.199 g/cc

@Temperature 5.00 °C
0.04332 lb/in³

@Temperature 41.0 °F
1.206 g/cc

@Temperature 0.000 °C
0.04357 lb/in³

@Temperature 32.0 °F
1.93 g/cc

@Temperature 10.0 °C
0.0697 lb/in³

@Temperature 50.0 °F
Solubility in Water 1.5 %
1.5 %
in organic
6.5 %
6.5 %
Viscosity 0.42 cP

@Temperature 120 °C
0.42 cP

@Temperature 248 °F
0.44 cP

@Temperature 110 °C
0.44 cP

@Temperature 230 °F
0.48 cP

@Temperature 100 °C
0.48 cP

@Temperature 212 °F
0.52 cP

@Temperature 90.0 °C
0.52 cP

@Temperature 194 °F
0.57 cP

@Temperature 80.0 °C
0.57 cP

@Temperature 176 °F
0.62 cP

@Temperature 70.0 °C
0.62 cP

@Temperature 158 °F
0.69 cP

@Temperature 60.0 °C
0.69 cP

@Temperature 140 °F
0.76 cP

@Temperature 50.0 °C
0.76 cP

@Temperature 122 °F
0.84 cP

@Temperature 40.0 °C
0.84 cP

@Temperature 104 °F
0.90 cP

@Temperature 35.0 °C
0.90 cP

@Temperature 95.0 °F
0.96 cP

@Temperature 30.0 °C
0.96 cP

@Temperature 86.0 °F
1.03 cP

@Temperature 25.0 °C
1.03 cP

@Temperature 77.0 °F
1.12 cP

@Temperature 20.0 °C
1.12 cP

@Temperature 68.0 °F
1.21 cP

@Temperature 15.0 °C
1.21 cP

@Temperature 59.0 °F
1.31 cP

@Temperature 10.0 °C
1.31 cP

@Temperature 50.0 °F
1.43 cP

@Temperature 5.00 °C
1.43 cP

@Temperature 41.0 °F
1.55 cP

@Temperature 0.000 °C
1.55 cP

@Temperature 32.0 °F
Molecular Weight 92.53 g/mol
92.53 g/mol
Vapor Pressure 0.00456 bar

@Temperature 0.000 °C
3.42 torr

@Temperature 32.0 °F
19 g/m<sup>3</sup> concentration of saturated vapor
0.00648 bar

@Temperature 5.00 °C
4.86 torr

@Temperature 41.0 °F
26 g/m<sup>3</sup> concentration of saturated vapor
0.00882 bar

@Temperature 10.0 °C
6.61 torr

@Temperature 50.0 °F
35 g/m<sup>3</sup> concentration of saturated vapor
0.0122 bar

@Temperature 15.0 °C
9.12 torr

@Temperature 59.0 °F
47 g/m<sup>3</sup> concentration of saturated vapor
0.0165 bar

@Temperature 20.0 °C
12.4 torr

@Temperature 68.0 °F
63 g/m<sup>3</sup> concentration of saturated vapor
0.0220 bar

@Temperature 25.0 °C
16.5 torr

@Temperature 77.0 °F
82 g/m<sup>3</sup> concentration of saturated vapor
0.0290 bar

@Temperature 30.0 °C
21.7 torr

@Temperature 86.0 °F
107 g/m<sup>3</sup> concentration of saturated vapor
0.0379 bar

@Temperature 35.0 °C
28.4 torr

@Temperature 95.0 °F
137 g/m<sup>3</sup> concentration of saturated vapor
0.0491 bar

@Temperature 40.0 °C
36.9 torr

@Temperature 104 °F
174 g/m<sup>3</sup> concentration of saturated vapor
0.0798 bar

@Temperature 50.0 °C
59.9 torr

@Temperature 122 °F
275 g/m<sup>3</sup> concentration of saturated vapor
0.126 bar

@Temperature 60.0 °C
94.2 torr

@Temperature 140 °F
420 g/m<sup>3</sup> concentration of saturated vapor
0.192 bar

@Temperature 70.0 °C
144 torr

@Temperature 158 °F
622 g/m<sup>3</sup> concentration of saturated vapor
0.285 bar

@Temperature 80.0 °C
214 torr

@Temperature 176 °F
898 g/m<sup>3</sup> concentration of saturated vapor
0.412 bar

@Temperature 90.0 °C
309 torr

@Temperature 194 °F
1264 g/m<sup>3</sup> concentration of saturated vapor
0.583 bar

@Temperature 100 °C
437 torr

@Temperature 212 °F
1739 g/m<sup>3</sup> concentration of saturated vapor
0.807 bar

@Temperature 110 °C
605 torr

@Temperature 230 °F
2344 g/m<sup>3</sup> concentration of saturated vapor
1.09 bar

@Temperature 120 °C
821 torr

@Temperature 248 °F
3101 g/m<sup>3</sup> concentration of saturated vapor
Surface Tension 0.035 dynes/cm
0.035 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 420 J/g

@Temperature 120 °C
181 BTU/lb

@Temperature 248 °F
Latent
427 J/g

@Temperature 110 °C
184 BTU/lb

@Temperature 230 °F
Latent
435 J/g

@Temperature 100 °C
187 BTU/lb

@Temperature 212 °F
Latent
442 J/g

@Temperature 90.0 °C
190 BTU/lb

@Temperature 194 °F
Latent
449 J/g

@Temperature 80.0 °C
193 BTU/lb

@Temperature 176 °F
Latent
456 J/g

@Temperature 70.0 °C
196 BTU/lb

@Temperature 158 °F
Latent
462 J/g

@Temperature 60.0 °C
199 BTU/lb

@Temperature 140 °F
Latent
469 J/g

@Temperature 50.0 °C
202 BTU/lb

@Temperature 122 °F
Latent
Electrical Properties Metric English Comments
Dielectric Constant 20.8

@Temperature 21.5 °C
20.8

@Temperature 70.7 °F
liquid
Chemical Properties Metric English Comments
Critical Pressure 49.0 bar
36800 torr
Critical Temperature 327 °C
621 °F
Copyright © lookpolymers.com All Rights Reserved