Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.700 g/cc @Thickness 1.00 - 6.00 mm |
0.0253 lb/in³ @Thickness 0.0394 - 0.236 in |
ASTM D792 |
CPC - Vycom CELTEC® Expanded Rigid foam PVC board Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface.. |
|||
Density | 0.702 g/cc @Temperature 260 °C |
0.0253 lb/in³ @Temperature 500 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |