Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.702 g/cc @Temperature 260 °C |
0.0253 lb/in³ @Temperature 500 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |