Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 934NA Paste Adhesive System Two part adhesive system with superior strengthCures at room temperatureApplications: Potting Structural Repair Liquid Shim |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9377 Paste Adhesive System Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9380.05 Paste Adhesive System High degree of cure after a low temperature cure time that offers strength, toughness and high temperature resistance of heat curing film adhesives with greater flexibility and ease of use. Can be a.. |
|||
Storage Temperature | <= 4.00 °C | <= 39.2 °F | 6 months |
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material.. |
|||
Storage Temperature | 4.00 °C | 39.2 °F | 12 months |
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed.. |
|||
Storage Temperature | <= 4.00 °C | <= 39.2 °F | 12 months |
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C.. |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9323 Paste Adhesive System Viscous, but pourable, liquid adhesive that yields tough, durable adhesive bonds over a wide temperature range.Application: Structural Repair |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9380 Paste Adhesive System Cures at low temperature. Offers strength, toughness and high temperature resistance of heat-curing film adhesives, with greater flexibility and ease of use. Can be applied to large parts with contr.. |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9396.6MD Paste Adhesive System Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic |
|||
Storage Temperature | <= 4.00 °C | <= 39.2 °F | 12 months |
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section .. |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |
|||
Storage Temperature | 4.00 °C | 39.2 °F | |
Henkel Hysol EA 956 Paste Adhesive System Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up |