Henkel Hysol EA 9380.05 Paste Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9380.05 Paste Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High degree of cure after a low temperature cure time that offers strength, toughness and high temperature resistance of heat curing film adhesives with greater flexibility and ease of use. Can be applied to large parts via a controlled meter mix operation or via dual cartridge static mixer kits.Applications: Structural Repair Composite Bonding Liquid Shim
Physical Properties Metric English Comments
Storage Temperature 4.00 °C
39.2 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 23.3 MPa

@Temperature 93.0 °C
3380 psi

@Temperature 199 °F
Tensile Lap Shear
27.8 MPa

@Temperature -55.0 °C
4030 psi

@Temperature -67.0 °F
Tensile Lap Shear
35.8 MPa

@Temperature 25.0 °C
5190 psi

@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 6.76 kN/m
38.6 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
120 min

@Temperature 80.0 °C
2.00 hour

@Temperature 176 °F
Pot Life 300 min
300 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 2266:1
Peel Strength High