Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9396.6MD Paste Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9396.6MD Paste Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic
Physical Properties Metric English Comments
Density 0.600 g/cc
0.0217 lb/in³
Storage Temperature 4.00 °C
39.2 °F
Mechanical Properties Metric English Comments
Compressive Strength 26.2 MPa
3800 psi
Adhesive Bond Strength 10.3 MPa

@Temperature 93.0 °C
1490 psi

@Temperature 199 °F
Tensile Lap Shear
13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Lap Shear
18.0 MPa

@Temperature 25.0 °C
2610 psi

@Temperature 77.0 °F
Tensile Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 82.0 °C
1.00 hour

@Temperature 180 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 120 min
120 min
Descriptive Properties Value Comments
Consistency Syntactic
Form 2 parts
Mix Ratio, Part A:Part B 100:31
Peel Strength Nil