Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | <= 50.0 °C | <= 122 °F | |
Dow Corning SYL-OFF® 23-30% COATING Syl-Off® 23 Paper Coating 30 Percent is a 30% active solids dispersion of silanol functional silicone polymers and multifunctional crosslinkers in xylene.Information provided by Dow Corning |
|||
Storage Temperature | <= 50.0 °C | <= 122 °F | |
Dow Corning SYL-OFF® 292 COATING Syl-Off® 292 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 30 percent solids dispersion of a blend of reactive siloxa.. |
|||
Storage Temperature | <= 50.0 °C | <= 122 °F | |
Dow Corning SYL-OFF® 294 COATING Syl-Off® 294 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 40 percent solids dispersion of a blend of reactive silox.. |
|||
Storage Temperature | <= 50.0 °C | <= 122 °F | |
Dow Corning SYL-OFF® C4-2109 RELEASE ADDITIVE C4-2109 is a 10% active solids solution of a silicate based compound. This product is recommended for use as a release modifier for Syl-Off® brand solvent based, condensation curing, systems.Inform.. |
|||
Storage Temperature | <= 50.0 °C | <= 122 °F | |
Dow Corning SYL-OFF® C4-2117 FAST CURE ADDITIVE Syl-Off® C4-2117 Fast Cure Additive is a 30% active solids silicate based compound. This product is recommended for use as a fast cure additive when used in conjunction with an organo-tin functiona.. |