Dow Corning SYL-OFF® 294 COATING

Category Fluid , Solvent
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® 294 COATING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® 294 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 40 percent solids dispersion of a blend of reactive siloxane polymers in VM&P naphtha.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.850 g/cc

@Temperature 25.0 °C
0.850 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 4000 cSt

@Temperature 25.0 °C
4000 cSt

@Temperature 77.0 °F
Storage Temperature <= 50.0 °C
<= 122 °F
Thermal Properties Metric English Comments
Flash Point >= 26.0 °C
>= 78.8 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 40
Appearance clear liquid
Color slightly hazy
Solvent VM&P naphtha