Material Notes:
Syl-Off® 292 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 30 percent solids dispersion of a blend of reactive siloxane polymers in xylene.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 25.0 °C
0.900 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 190 cSt

@Temperature 25.0 °C
190 cSt

@Temperature 77.0 °F
Storage Temperature <= 50.0 °C
<= 122 °F
Thermal Properties Metric English Comments
Flash Point >= 28.0 °C
>= 82.4 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 5.00 Month
5.00 Month
Descriptive Properties Value Comments
Active Content (%) 30
Appearance clear liquid
Color slightly hazy
Solvent xylene